silverfence.com silverfence.com silverfence.com
   Main Page -> About Us -> Security & Privacy -> Terms of Use -> Add Your Link -> Add Article
Search:   
Add Url
 

Technology & Science

Automobiles

Eating & Drinking

Adventure & Sports

Business & Commerce

Finance & Investment

Academics & Learning

Internet & Computers

Online & Board Games

Realty & Property

Relationship & Lifestyle

Health & Therapy

Medical Care

Culture & Art

Law & Politics

Teens & Kids

Employment & Careers

Events & News

Travel & Vacation

Self Healing

Home & Garden

People & Communities

Recreation

Online Shopping

 

Main Page –› Academics & Learning –› Pure Sciences
 

Reversing Mother Nature, Part Two

 

ISL EXTRACTION AND PROCESSING

During ISL mining, water is pumped to the surface from production wells that contain uranium in very low concentrations, on the order of parts per million concentrations. The next step in the ISL process is to extract the uranium dicarbonate. Extraction is done by chemically exchanging ions inside a processing facility. The ion exchange process is very analogous to a home Culligan water softener, Anthony revealed. It removes hardness or calcium from the water by replacing it with sodium, using ion exchange resins. If you go to Lowes or Home Depot, and buy a water softener, you basically have a home version of a uranium extraction plant. The main difference is your water softener will have a cation exchanger. For a uranium plant to function properly, you need to use an anion exchange resin, which is specifically designed to load uranium, Anthony clarified.

And what is this magical ion exchange resin? The resin is comprised of little polymer beads, which are charged particles having an affinity for uranium anions. There are literally millions of these small resin beads in a vessel, which can adsorb low concentration of uranium in solution, said Anthony. Adsorption is when something is attracted to something else or clings to it, like static electricity.

Why do you have to process uranium like this? In essence, the ion exchange process is a beneficiation (reduction) process that concentrates large volumes of low concentrate uranium solution into a much smaller volume containing a much higher concentration of uranium, said Anthony. In other words, the beneficiation is just concentrating the uranium from the large volume of water in which it is mined into a more compact form. The preferred means is through an ion exchange.

Anthony gave a real-life example of the beneficiation process, Three million gallons of wellfield solution containing dilute concentrations of uranium, of 100 parts per million minus 0.10 grams/liter, is passed through a bed of ion exchange resin. This might take 24 hours to achieve if the solution is flowing at 2,500 gallons per minute. After this length of time, the resin becomes loaded with approximately 2,500 pounds of uranium.

STRIPPING THE URANIUM

Stripping the uranium is called the elution process. This is done through a chemical exchange of positively and negatively charged ions. Resins are classified by the charge on the active sites. The active sites on the resin are positively charged for anion resins and negatively charged for cation resins, Norris enlightened us. The resins ability to extract chemical ions from a solution is derived from whats called an active site, he continued. In our case, chloride ions obtained from ordinary tale salt are used to stabilize or temporarily neutralize this positively charged active site. The negatively charged chloride ion sticks to the positively charged site, held in place by what Norris called electrostatic forces. When the negatively charged ions, such as uranyl dicarbonate, are placed in contact with the solution, it will kick off the chloride and replace that with the uranyl dicarbonate.

That was the chemistry lesson. Anthony summed it up in a nutshell, They just displace it. Theres a greater affinity for the chloride ion to the resin than there is for the uranium. So, the uranium is stripped from the resin bed. The processing facility chemically strips the loaded uranium from the resin by soaking the entire package of uranium-laden resin in a salt bath solution. The volume of salt solution is on the order of 10,000 gallons resulting in a solution concentration of 30 grams/liter uranium, Anthony said, describing the process of how the uranium becomes concentrated. The stripped uranium solution concentration is magnified 300 times more than the wellfield solution, he informed us. The concentration level can now be economically processed for recovery: precipitation, dewatering, drying and drumming for a nuclear facility.

GETTING URANIUM INTO THE DRUM

After the uranium has been removed from the solution, it is precipitated. At this point in the processing stage, you have yellowcake slurry. Up close, it looks like a sort of yellowish and wet, runny cement mixture. The dewatering process does just that, it removes the water from the yellowcake mixture.

I use a filter press, a device that is designed to separate solids from solutions, explained Anthony. Filter presses are extensively used in various types of food, chemical and drug processing across the world. The uranium solids, now looking more like yellowcake, are retained in the filter press, where they can be washed and later air dried, before drying them to a powder with a low temperature vacuum dryer, said Anthony taking us step by step through this process.

So what is the filter press and how do you end up with the finished yellowcake when youre done? Its a series of plates and hollow frames, or it could be a series of recessed chambers, Anthony answered. Filter cloth is draped over the plates or chalked in the recessed chambers. The yellowcake slurry is pumped through the filter allowing the liquid phase to pass through the filter cloth, trapping the uranium oxide inside the device. Anthony likes to pack the filter press up with as much yellowcake as it can hold. It is then washed with clean water to displace the chloride ions to a low level, Anthony explained. If you dont remove the chloride concentrations to the acceptable level required by an uranium enrichment facility, a fine is assessed against that shipment.

The final steps include conveying the yellowcake to the vacuum dryer. The uranium oxides color depends on how high or low a temperature is used to dry the yellowcake. Patrick Drummond, the Smith-Highland Ranch plant superintendent, showed us pure uranium oxide dried at high temperatures. It was nearly black. After the drying process is complete, the uranium is packaged up in DOE-approved 55 gallon drums and transported to an enrichment facility. It is then when the enriched uranium can finally be used to power a nuclear reactor and provide an inexpensive source of electricity.

Author: James Finch
 
Author Bio:
James Finch is a popular columnist. James likes to pen down articles about this area.
 
 
 

Related Articles

 
All About Anna Salleh's Beat Up, And Questions She Should Have Asked Associate Professor Jack Heinem
 
Do You Think This 145 Year Old System Still Works Today?
 
Ergonomic Positioning Explained: Part Two, Your Spine
 
Holistic Approach May Be The Key to Curing Addiction
 
How To Protect Yourself Fom Online Education Degree Scams
 
An Insight into the Problem of Stammering
 
On the Shelf-A Book Review
 
Some Helpful Advice for Non-Native English Speaking English EFL / ESL Teachers
 
The Quintessential Urban Lullaby: a Review of "Black Cat"
 
IT Certification Exams: 3 Most Popular Mistakes
 
 
 
Main Page -> Security & Privacy -> Terms of Use  
© 2006-2008 www.silverfence.com All Rights Reserved Worldwide.